Title :   THE EFFECT OF SURFACE DECARBURIZATION ON PROTOTYPE MISSILE CASES.

Descriptive Note : Quarterly rept. no. 1, 1 Jan-30 Jun 62,

Corporate Author : INGERSOLL KALAMAZOO DIV BORG-WARNER CORP

Personal Author(s) : Mills ,E. S. ; Thomason,D. P.

Report Date : 20 JUL 1962

Pagination or Media Count : 20

Abstract : The materials used in the program are 2 steels, MBMC ?1 and super tricent. Drawings of the prototype cases as well as the bonded uniaxial and biaxial stress specimens are shown. Test results are presented for the first group of tensile specimens having a bonded lap joint. Average joint strength for the group was 15,860 lb per peripheral inch (width), somewhat above the target joint strength of 15,000 established for the prototype bonded end ring case. A curve is drawn showing the hydrotest pressures for various size missile cases a bonded joint of this strength will withstand. (Author)

Descriptors :   (*CARBON), (*STEEL), (*ROCKET CASES), WELDED JOINTS, JOINTS, ADHESIVES, SHEAR STRESSES, DISPOSAL, BONDED JOINTS, BONDING, MANUFACTURING, PIPES, PRESSURE, SURFACES, TENSILE PROPERTIES

Distribution Statement : APPROVED FOR PUBLIC RELEASE