Title :   METHOD OF OBTAINING LUBRICANT FOR HOT WORKING OF METALS,

Corporate Author : FOREIGN TECHNOLOGY DIV WRIGHT-PATTERSON AFB OHIO

Personal Author(s) : Kalinkina,Z. M. ; Evsyukova,G. A.

Report Date : 21 OCT 1965

Pagination or Media Count : 6

Abstract : The object of the invention is a method for obtaining lubricant for hot working of metals by means of a mixture of emulsion, graphite, and glass. For the purpose of increasing the interval of softening and the heat resistance of the lubricant one uses glass consisting of 13.8 to 14 percent of silicon oxide, 10 to 10.12 percent of boron oxide, 49 to 49.2 percent of potassium oxide, 17.78 to 18 percent of sodium oxide, and 9 to 9.1 of iron oxide. (Author)

Descriptors :   (*HOT WORKING, LUBRICANTS), (*LUBRICANTS, HOT WORKING), USSR, PATENTS, GLASS, GRAPHITE, OXIDES, SILICON COMPOUNDS, BORON COMPOUNDS, POTASSIUM, SODIUM COMPOUNDS, IRON COMPOUNDS, COLLOIDS

Subject Categories : Ceramics, Refractories and Glass