Title :   WHITE OAK LAMINATES COMPARISON OF 12-DAY AND 3-HOUR DELINATION TEST RESULTS.

Descriptive Note : Development rept.,

Corporate Author : PUGET SOUND NAVAL SHIPYARD BREMERTON WASH MATERIAL LABS

Personal Author(s) : Stahl,E.

Report Date : JAN 1960

Pagination or Media Count : 19

Abstract : Correlation studies between the 12-day cyclical exposure test of Specification MIL-W-0015154B and a proposed 3-hour delamination test were made on white oak face laminates. Results indicated the 3-hour test method to be suitable for quality control purposes. A limited number of values were also obtained on scarf joints. (Author)

Descriptors :   (*LAMINATES, WOOD), (*QUALITY CONTROL, LAMINATES), TEST METHODS, DEGRADATION, JOINTS, AGING(MATERIALS), SPECIFICATIONS, MILITARY REQUIREMENTS

Subject Categories : Laminates and Composite Materials
      Wood, Paper and Related Forestry Products