Accession Number : AD0828493

Title :   ON THE INFLUENCE OF SMALL AMOUNTS OF SUBSTITUTIONAL ELEMENTS ON RECOVERY RECRYSTALLIZATION AND INTERNAL FRICTION OF HIGH-PURITY IRON. NOTE III.

Descriptive Note : Technical rept. (Final),

Corporate Author : NATIONAL ELECTROTECHNICAL INST TURIN (ITALY)

Personal Author(s) : Venturello, C. ; Antoione, C. ; Della Gatta, G. ; Lucci, A. ; Riontino, R.

Report Date : OCT 1967

Pagination or Media Count : 83

Abstract : Continuing the research work on the effect of small amounts of substitutional transition elements on recrystallization, recovery and grain boundary relaxation in iron, data obtained for a new set of iron alloys containing Co, Mn, Ga and Ge (contents ranging from 40 to 1075 atoms per million) are reported. A discussion concerning also the results previously obtained (for alloys with Ti, V, Co, Ni, Cu) is given.

Descriptors :   (*IRON ALLOYS, MECHANICAL PROPERTIES), CHROMIUM, MANGANESE, GALLIUM, GERMANIUM, TITANIUM, VANADIUM, COBALT, NICKEL, COPPER, RECOVERY, RECRYSTALLIZATION, INTERNAL FRICTION, IMPURITIES, HARDNESS, ANNEALING, GRAIN BOUNDARIES, ITALY.

Subject Categories : Metallurgy and Metallography

Distribution Statement : APPROVED FOR PUBLIC RELEASE