Accession Number : ADA298896

Title :   IR Materials Producibility.

Descriptive Note : Final rept. 12 Aug 92-11 Sep 95,

Corporate Author : SRI INTERNATIONAL MENLO PARK CA

Personal Author(s) : Berding, M. A., Sr. ; Sher, A.

PDF Url : ADA298896

Report Date : SEP 1995

Pagination or Media Count : 170

Abstract : SRI International is submitting the Final Technical Report entitled "IR Material Producibility" for the referenced contract. Auto-compensation by isolated native point defects is not responsible for the type doping limitations in ZnSe-based materials. Excess generation of Frenkel defects at stacking faults is responsible for the operational degradation of ZnSe-based LEDs and lasers. (MM)

Descriptors :   *OPTICAL MATERIALS, *SEMICONDUCTORS, *DEFECTS(MATERIALS), *INFRARED SPECTRA, DENSITY, DEGRADATION, LASERS, POINT DEFECTS, INTERSTITIAL, TRANSPORT PROPERTIES, CADMIUM TELLURIDES, DOPING, STACKING, MERCURY CADMIUM TELLURIDES, LIGHT EMITTING DIODES, ZINC SELENIDES.

Subject Categories : Electrical and Electronic Equipment
      Optics

Distribution Statement : APPROVED FOR PUBLIC RELEASE