Title :   Flame Cutting of Armor - 1 Inch Rolled Homogeneous Armor (0.30% C),

Corporate Author : WATERTOWN ARSENAL MA

Personal Author(s) : Herres,S. A. ; Warner,W. L.

Report Date : 02 NOV 1942

Pagination or Media Count : 10

Abstract : The object of the U/A report was to determine the maximum hardness developed by flame cutting armor plate of 0.30% carbon grade at room temperature, and to determine the preheat necessary to reduce this hardness to 400 Brinell. The maximum hardness developed in flame affected area in armor plate of compositions investigated when flame cut at room temperature is approximately 500 Brinell. A preheat of 400 F. is sufficient to limit this maximum hardness to 400 Brinell.

Descriptors :   ARMOR, ARMOR PLATE, CUTTING, FLAMES, HOMOGENEITY, ROLLING(METALLURGY), ROOM TEMPERATURE, TORCHES