Title :   Gold-Tin-Silicon Alloy for Brazing Silicon to Metal.

Descriptive Note : Patent,

Corporate Author : DEPARTMENT OF THE AIR FORCE WASHINGTON DC

Personal Author(s) : Kitchen,Donald R ; Jacobson,Loren A

Report Date : 29 Jul 1980

Pagination or Media Count : 4

Abstract : An alloy for brazing a silicon die to a gold-plate kovar header consists essentially of 19 to 21 weight percent tin and 0.6 to 0.8 weight percent silicon with the balance being gold. The alloy melts at a temperature below 200 C. which is substantially lower than that of the conventional gold-silicon eutectic alloy. (Author)

Descriptors :   *Patents, *Brazing, *Silicon alloys, Gold alloys, Tin alloys, Plating, Melting point, Eutectics, Inventions, Substrates, Bonding, Integrated circuits, Dies