Abstract : A high rate carbon cathode is made by mixing a carbon powder having a surface area of about 1000 square meters/gram with polytetrafluoroethylene and a sufficient amount of water to form a coherent mixture. The mixture is applied to an electrically conductive screen; the cathode formed while wet to an intermediate thickness, the cathode vacuum dried at about 100 degrees C, and the cathode cold compressed to obtain a final electrode porosity of greater than 80 percent. The cathode can be used in a lithium primary cell using a solution of an inorganic lithium salt in sulfuryl chloride as the electrolyte. (Author)

Descriptors :   *Patent applications, *Cathodes(Electrolytic cell), *Carbon black, Electrodes, Thickness, Porosity, Foils(Materials), Lithium alloys, Separation, Fabrication, Aluminum compounds, Chlorides, Drying

Subject Categories : Electrical and Electronic Equipment

Distribution Statement : APPROVED FOR PUBLIC RELEASE